Short answer: what is crocking (rubbing fastness)

Crocking (rubbing fastness) is dye that transfers from a fabric onto skin or another material when they rub together — for example, a dark uniform marking a light inner shirt over a working day. It is measured under ISO 105-X12 or AATCC 8: a machine rubs a white cotton swatch over the sample, and the staining on the swatch is rated 1–5 on a grey scale (5 = no transfer at all)

Why dark fabric marks more

  • Dark shades carry more dye — so more unfixed dye sits on the fibre surface
  • Fixation decides — if the dye is not fully bonded to the fibre, friction carries it away
  • Wet conditions make it worse — water helps dye molecules migrate onto the other surface
  • Light colours carry less dye — so they crock less by nature
  • Note: crocking is a surface-fixation problem — a fabric can pass washing fastness yet still crock if surface dye is not fixed

How a crocking test works (ISO 105-X12 / AATCC 8)

  1. A white cotton test swatch (desized, bleached, unfinished) is cut into squares of about 50 mm
  2. A crockmeter rubs the swatch back and forth over the sample under standard pressure (about 9 N) for 20 rubs
  3. Two tests — dry rubbing (dry swatch) and wet rubbing (swatch soaked in water)
  4. The staining on the swatch is graded with a grey scale (ISO 105-A03): 5 = no staining · 4 = very slight · 3 = slight · 2 = distinct · 1 = heavy

Dry rubbing vs wet rubbing

  • Dry — measures staining in normal wear: friction against skin, seats and furniture
  • Wet — usually grades lower, because water helps the dye migrate; important for workwear that sweats or gets wet

ISO 105-X12 vs AATCC 8

  • Same principle: crockmeter + white cotton swatch + grey scale
  • They differ in swatch size, applied force and soak level (ISO wet rubbing about 100% uptake · AATCC about 65%)
  • Results under the two standards are not always identical for every shade — the spec should name which standard applies

What crocking grade is acceptable

  • There is no single mandatory number for every use — state the required grade + standard + test condition in the spec, e.g. "dry rubbing, grade 4, per ISO 105-X12"
  • Light shades can usually be specified at a higher grade; dark shades such as navy or black are commonly specified one notch lower
  • With the same standard and method, grades are comparable across lots — which is exactly why the spec must name the method

How a dyeing mill keeps crocking low

  • Dye to the target shade and fix the dye completely — disperse dyed at full heat until it enters the fibre, reactive fixed with alkali to recipe
  • Soaping — washing unfixed dye out of the fibre at heat with detergent
  • Finishing steps that add no new dye and do not loosen the surface colour
  • QC and testing on every lot — including an in-house rubbing test

Boonchuay Industrial: crocking tested in our own lab

Boonchuay Industrial (BCI) is a dyeing and finishing mill with over 60 years of experience in Nakhon Pathom. Our in-house lab runs the rubbing test (crocking) alongside the rest of the colour-fastness panel:

  • Tests to ISO, JIS, AATCC and Daimaru methods
  • Lab dyeing that duplicates the factory's real production process (both batch and continuous)
  • Three QC checkpoints — greige inspection before dyeing, in-process control and inspection at packing
  • 10-point quality report with every lot
  • MOQ is negotiable — depends on process, colour and order size

See fabric dyeing from a dyeing mill · our standards and quality control · or contact us

FAQ

Q: What does a crocking grade of 4 mean? A: On the 1–5 scale, 4 = "very slight" transfer — the staining on the swatch is barely visible; 5 = no staining at all. Buyers commonly specify 4 or better for uniforms and apparel.

Q: Does crocking disappear after a few washes? A: If the staining comes from surface dye that was not fixed, proper washing can reduce crocking over washes — but buyers specify the crocking grade from the first lot, not after customer washes.

Q: Which matters more, dry or wet rubbing? A: It depends on the end use — everyday wear and uniforms focus on dry rubbing; workwear that sweats or gets wet should be checked on both, since wet crocking usually grades lower.

Q: If it passes washing fastness, can it still crock? A: Yes — they are different tests. Washing fastness (ISO 105-C06 / AATCC 61) measures colour change after washing; crocking (ISO 105-X12 / AATCC 8) measures transfer by rubbing. A fabric can pass washing and still crock.

Q: How do I specify crocking in a spec sheet? A: Three parts — the grade required (e.g. 4), the standard (ISO 105-X12 dry rubbing), and the test conditions. A dyeing mill testing to the same standard gives results you can compare across lots.

References

  1. ISO 105-X12:2016 Textiles — Tests for colour fastness — Part X12: Colour fastness to rubbing — ISO
  2. Color Fastness to Rubbing Test Method — Textile Learner
  3. TM008 Test Method for Colorfastness to Crocking — AATCC
  4. Test Methods and Standards — AATCC